Methods of test for pulp and paper Removal of latency
出版:Standards Australia

專家解讀視頻
This standard sets out a method for the removal of latency from all high yield pulps that have been produced at elevated temperature and cooled before the concentration is reduced. The method involves disintegration at low consistency and elevated temperature followed by rapid cooling to an even lower consistency. To ensure rapid cooling, the use of ice is recommended.