UNI EN 12697-4:2005現(xiàn)行

Bituminous Mixtures - Test Methods For Hot Mix Asphalt - Part 4: Bitumen Recovery: Fractionating Column

出版:Italian Standards

獲取原文 如何獲取原文?問客服 獲取原文,即可享受本標(biāo)準(zhǔn)狀態(tài)變更提醒服務(wù)!

專家解讀視頻

基本信息
標(biāo)準(zhǔn)編號: UNI EN 12697-4:2005
標(biāo)準(zhǔn)類別:Standard
出版單位:Italian Standards
標(biāo)準(zhǔn)頁數(shù):0
標(biāo)準(zhǔn)簡介

Defines a test method for the recovery of soluble bitumen from bituminous mixtures from pavements in a form suitable for further testing. Suitable for the recovery of paving grade bitumen and for mixtures containing volatile matter such as cut-back bitumen but results may be less precise.

等同采用的國際標(biāo)準(zhǔn)

BS EN 12697-4:2005 - Identical

SN EN 12697-4:2005 - Identical

SN EN 12697-4:2016 - Identical

UNE EN 12697-4:2015 - Identical

SS EN 12697-4 Ed. 3 (2015) - Identical

BS EN 12697-4:2015 - Identical

NF EN 12697-4:2015 - Identical

EN 12697-4:2015 - Identical

DIN EN 12697-4 (2005-04) - Identical

NBN EN 12697-4:2005 - Identical

UNE EN 12697-4:2006 - Identical

SS EN 12697-4 Ed. 2 (2005) - Identical

NEN EN 12697-4:2005 - Identical

ONORM EN 12697-4:2005 - Identical

NF EN 12697-4:2005 - Identical

I.S. EN 12697-4:2005 - Identical

NS EN 12697-4 Ed. 2 (2005) - Identical